Evaporated and sputtered thin films
Tighe, N. J., Fryer, J. R. and Flower, H. M.  International Tables for Crystallography (2006). Vol. C, Section 3.5.1.5, p. 173 [ doi:10.1107/97809553602060000589 ]
Evaporated and sputtered thin films 3.5.1.5. Evaporated and sputtered thin films Thin nonmetallic films are prepared by electron-beam heating and by plasma sputtering for direct applications such as optical and dielectric films and for standard samples for calibration of the X-ray and electron-energy-loss element-analysis spectrometers on ...

Final thinning by chemical etching
Tighe, N. J., Fryer, J. R. and Flower, H. M.  International Tables for Crystallography (2006). Vol. C, Section 3.5.1.4, p. 173 [ doi:10.1107/97809553602060000589 ]
... garnet (YAG). J. Sci. Instrum. 44, 862-863. Kirkpatrick, H. B. & Amelinckx, S. (1962). Device for chemically thinning crystals ... transmission electron microscopy. Rev. Sci. Instrum. 33, 488-489. Lewis, M. H. (1966). Defects in spinel crystals grown by the ...

Final thinning by argon-ion etching
Tighe, N. J., Fryer, J. R. and Flower, H. M.  International Tables for Crystallography (2006). Vol. C, Section 3.5.1.3, pp. 172-173 [ doi:10.1107/97809553602060000589 ]
... of materials. Mater. Res. Soc. Symp. 254, 43-63. Bach, H. (1964). Elektronenmikroskopische Durchstrahlungsaufnahmen und Feinbereichselektronenbeugung an Al2O3 Keramik. BOSCH Techn. Ber. 1, 10-13. Drum, C. M. (1965). Electron microscopy of dislocations and other defects in ... thinned by sputtering. Phys. Status Solidi, 9, 635-642. Paulus, M. & Reverchon, F. (1961). Dispositif de bombardement inonique pour ...

Thin-section preparation
Tighe, N. J., Fryer, J. R. and Flower, H. M.  International Tables for Crystallography (2006). Vol. C, Section 3.5.1.2, pp. 171-172 [ doi:10.1107/97809553602060000589 ]
... for the analysis. Typical petrographic sections are 100 to 200m thick. Disc-shaped specimens are cut from the petrographic thin ... sections can be ground and polished as thin as 30m before ion thinning, experience has shown that such thin discs ... can be ground and polished to a thickness of 50m by the use of various grades of abrasive. With ...

Thin fragments, particles, and flakes
Tighe, N. J., Fryer, J. R. and Flower, H. M.  International Tables for Crystallography (2006). Vol. C, Section 3.5.1.1, p. 171 [ doi:10.1107/97809553602060000589 ]
... materials science. Practical methods in electron microscopy, edited by A. M. Glauert, pp. 3-180. Amsterdam: North-Holland. Zvyagin, B. B. ...

Ceramics and rock minerals
Tighe, N. J., Fryer, J. R. and Flower, H. M.  International Tables for Crystallography (2006). Vol. C, Section 3.5.1, pp. 171-173 [ doi:10.1107/97809553602060000589 ]
... for the analysis. Typical petrographic sections are 100 to 200m thick. Disc-shaped specimens are cut from the petrographic thin ... sections can be ground and polished as thin as 30m before ion thinning, experience has shown that such thin discs ... can be ground and polished to a thickness of 50m by the use of various grades of abrasive. With ...